NOBIL-METAL® S.p.A. - DENTAL ALLOYS& SOLDERS

"A smile makes the difference."



New Cer Plus

White colour













Chemical composition

Au Pd Ag In Ga Ru Au&PGM
6.0% 74.7% 8.5% 3.5% 7.0%

X

81.0%

X=<1,0%


Technical data

Density g/cm³

10.9

Yield strength MPa

600 - 620

Melting range °C

1130 - 1240

Elongation %

30 - 15

Casting temperature°C

1390

Tensile strength MPa

700 - 800

TEC 25-500°C-25-600°C 10-6K-1

13.7 - 14.0

Vickers hardness HV5/30

290 - 300 - 340

Modulus of elasticity GPa

116

Crucible

ceramic